3M 5413

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 5413

Main features

  • Kapton Polyimide Backing
  • High-Temperature Silicone Adhesive
  • -73 to 260 deg C Use Range

Product Description

3M™ Polyimide Film Tape 5413 is an amber, 0.07 mm (2.7 mil) tape constructed with DuPont™ Kapton® polyimide film and silicone adhesive. It is used for printed circuit board solder masking and other high-temperature applications. The dimensionally stable polyimide backing does not soften at elevated temperatures and provides a release surface for high-temperature processing. The silicone adhesive supports high-temperature performance with reduced adhesive transfer, while the tape also provides documented flame-retardant, chemical-resistant, radiation-resistant, dielectric, and mechanical properties.

Key features

  • High-temperature polyimide backing: DuPont™ Kapton® film remains dimensionally stable and does not soften at elevated temperatures.
  • Silicone adhesive: Supports high-temperature processing while helping reduce adhesive transfer during removal.
  • Documented functional performance: Provides flame retardancy, chemical and radiation resistance, and a typical dielectric strength of 7,000 volts.

Applications / Suitable for

  • Masking gold fingers on printed circuit boards during wave soldering
  • Masking gold fingers during solder-dip processing
  • Providing a release surface during fabrication of parts cured at elevated temperatures
Product Family

3M 5413

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive LayerAdhesive Layer
Silicone
ColorColor
Amber
Film ThicknessFilm Thickness
0.03 mm
Release LinerRelease Liner
None
Total ThicknessTotal Thickness
70 μm
Mechanical Properties
ElongationElongation
62 %
Thermal Properties
Operating TemperatureOperating Temperature
-73° to 260°C °C
Electrical Properties
Breakdown VoltageBreakdown Voltage
7000 V

Additional Information

Technical properties

As-supplied / before-processing properties

Typical construction, dimensional, and storage properties of 3M™ Polyimide Film Tape 5413. Values are representative and are not intended for specification purposes.

Property Value Unit Method / condition
Backing DuPont™ Kapton® polyimide film — Typical construction
Adhesive Silicone — Typical construction
Color Amber — Typical
Backing thickness 1.0 (0.03) mil (mm) ASTM D-3652
Total tape thickness 2.7 (0.07) mil (mm) ASTM D-3652
Standard roll length 33 (36) m (yd) Standard roll format
Shelf life 36 months From date of manufacture when stored in original cartons at 21°C (70°F) and 50% relative humidity

 

Technical properties

After-processing / final-state properties

Typical mechanical, adhesion, electrical, thermal, and outgassing properties of 3M™ Polyimide Film Tape 5413. Values are representative and are not intended for specification purposes.

Property Value Unit Method / condition
Adhesion to steel 22 (24) oz/in width (N/100 mm) ASTM D-3330
Tensile strength at break 33 (578) lb/in width (N/100 mm) ASTM D-3579
Elongation at break 62 % ASTM D-3579
Temperature-use range -73 to 260 (-100 to 500) °C (°F) Typical temperature-use range
Dielectric strength 7,000 volts ASTM D-149
Total mass loss 1.50 % Outgassing result; %TML
Collected volatile condensable material 0.50 % Outgassing result; %CVCM
Flame retardancy Pass — UL 510 product category OARC2; File E124809

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers