ABLESTIK 342-3.5

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ABLESTIK 342-3.5

Main features

  • Two-Part Ambient-Cure Processing
  • 5,000 mPa s Application Viscosity
  • 29.0 N/mm^2 Aluminum Lap Shear

Product Description

LOCTITE® ABLESTIK 342-3.5 is a two-component amber epoxy adhesive for general assembly applications. It can cure at room temperature or with heat and is documented for bonding semi-porous materials such as ferrites where a physical bond is required. The adhesive provides a typical viscosity of 5,000 mPa·s at 25°C and an eight-hour work life at 25°C. Guideline cure options include 48 hours at 25°C, 4 hours at 75°C, 2 hours at 95°C, or 1 hour at 120°C. Typical cured properties include Shore D hardness of 86, a glass-transition temperature of 71°C, and aluminum-to-aluminum lap shear strength of 29.0 N/mm² at 25°C.

Key features

  • Room-temperature or heat cure: Guideline cure schedules range from 48 hours at 25°C to 1 hour at 120°C.
  • Extended working time: Typical work life is eight hours at 25°C, based on a 25% increase in viscosity.
  • High bonded-joint strength: Typical aluminum-to-aluminum lap shear strength is 29.0 N/mm² at 25°C.

Applications / Suitable for

  • General assembly bonding
  • Bonding semi-porous materials such as ferrites where a physical bond is required
  • Aluminum-to-aluminum bonding under the documented test condition
Product Family

ABLESTIK 342-3.5

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Amber
Chemistry TypeChemistry Type
Epoxy
Work life @25°CWork life @25°C
8 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
71 °C
Physical Properties
ViscosityViscosity
5000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical physical, handling, storage, and guideline cure information before final processing.

Property Value Unit Method / condition
Technology Epoxy — Two-component adhesive
Appearance Amber liquid / paste — TDS appearance and SDS physical-state description
Viscosity 5,000 mPa·s (cP) Brookfield CP51, 5 rpm at 25°C
Density / relative density 1.2 — SDS physical-property value
VOC content 2 g/L SDS value
Work life 8 hours At 25°C; endpoint is a 25% increase in viscosity
Shelf life — kits 365 days At 25°C, from date of manufacture
Shelf life — premixed frozen syringes 365 days At -40°C, from date of manufacture
Recommended cure schedule 48 hours At 25°C; guideline recommendation
Alternative cure schedules 4 hours, 2 hours, or 1 hour — 4 hours at 75°C, 2 hours at 95°C, or 1 hour at 120°C; guideline recommendations
Technical properties

After-processing / final-state properties

Typical physical, thermal, and bonded-joint properties of the cured adhesive. Values are reference data and are not product specifications.

Property Value Unit Method / condition
Hardness 86 Shore D Cure condition and test method not stated
Glass-transition temperature 71 °C Method and cure condition not stated
Coefficient of thermal expansion — below Tg 35 ppm/°C TMA; cure condition not stated
Coefficient of thermal expansion — above Tg 180 ppm/°C TMA; cure condition not stated
Lap shear strength — aluminum to aluminum 29.0 (4,200) N/mm² (psi) Tested at 25°C; surface preparation, bondline, cure condition, and test method not stated

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers