ABLESTIK SF 40

Harmonization Code : 5906100000 | Adhesive tape of a width not exceeding 20cm

ABLESTIK SF40

Main features

  • Low-Density Syntactic Foam Adhesive
  • Thixotropic Vertical-Surface Control
  • Room-Temperature Adhesive Cure

Product Description

LOCTITE® ABLESTIK SF 40 is a two-component, non-conductive epoxy adhesive formulated as a lightweight, low-density syntactic foam. The thixotropic, non-sag system is suitable for bonding and repairing vertical surfaces where limiting added weight is important. It mixes at 100:9 by weight and can be cured at room temperature or with heat. Documented applications include aerospace and hydrospace assemblies, with ceramics, metals, and plastics identified as key substrates. The cured adhesive has a documented operating-temperature range of -40 to 120°C.

Key features

  • Lightweight syntactic foam: Mixed density of 0.64 g/cm³ supports bonding and repair applications where added weight is a consideration.
  • Non-sag, thixotropic consistency: Supports application to vertical surfaces while helping the mixed adhesive remain in place before cure.
  • Flexible cure options: Cures in 48 to 72 hours at 25°C or in 2 to 4 hours at 65°C.

Applications / Suitable for

  • Aerospace applications
  • Hydrospace applications
  • Repairing vertical surfaces with limited added weight
  • Bonding ceramics, metals, and plastics
Product Family

ABLESTIK SF 40

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)Density (g)
0.64 g/cm3
Mix RatioMix Ratio
100 : 9
Work life @25°CWork life @25°C
0.5 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
107 °C
Operating TemperatureOperating Temperature
-40 to 120 °C
Chemical Properties
Water AbsorptionWater Absorption
2.0 %
Electrical Properties
Dielectric StrengthDielectric Strength
13.8 kV/mm
Volume ResistivityVolume Resistivity
1×10¹² Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the individual components and mixed adhesive before cure.

Property Value Unit Method / condition
Appearance — Part A White paste — As supplied
Appearance — Part B Amber liquid — As supplied
Mix ratio — Part A:Part B 100:9 by weight Two-component system
Density — Part A 0.61 g/cm³ ASTM D792
Viscosity — Part B 95 mPa·s (cP) Brookfield viscosity, ASTM D2393
Density — Part B 0.98 g/cm³ ASTM D792
Density — mixed adhesive 0.64 g/cm³ ASTM D792
Work life 30 minutes 100 g mixed quantity at 25°C
Shelf life 365 days At 25°C
Cure schedule 48–72 hours or 2–4 hours — 48–72 hours at 25°C or 2–4 hours at 65°C; guideline recommendations
Technical properties

After-processing / final-state properties

Typical properties and performance data for the cured adhesive. Values are reference data rather than product specifications.

Property Value Unit Method / condition
Operating-temperature range -40 to 120 °C Documented product range
Hardness 70 Shore D ASTM D2240
Water absorption 2.0 % ASTM D570
Coefficient of thermal expansion — below Tg 33 ppm/°C ASTM D3386
Coefficient of thermal expansion — above Tg 107 ppm/°C ASTM D3386
Glass-transition temperature 107 °C ASTM D3418
Dielectric strength 13.8 kV/mm ASTM D149
Dielectric constant / dissipation factor 2.5 / 0.02 — ASTM D150 at 1 mHz, as reported
Volume resistivity at 25°C 1 × 1012 ohm-cm ASTM D257
Total mass loss 0.23 % TML, ASTM E595
Collected volatile condensable material 0.04 % CVCM, ASTM E595
Tensile lap shear strength — aluminum to aluminum 14.5 (2,100) N/mm² (psi) Tested at 25°C
Tensile lap shear strength — aluminum to aluminum 12.4 (1,800) N/mm² (psi) Tested at 65°C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers