BONDERITE C-AK 5948-R

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-AK 5948-R

Main features

    Product Description

    BONDERITE® C-AK 5948 R EU AERO is a blue, water-based alkaline cleaner concentrate formulated for cleaning painted and unpainted aircraft exterior and interior surfaces after dilution with water. Suitable for aircraft metals and well-bonded paint, it provides nonstaining, nonstreaking cleaning on aluminum and rinses freely after use. The product is designed for immersion and dip applications, including ultrasonic parts-cleaning systems, and is suitable for all models of jet aircraft.

    Key features

    • Aircraft-surface compatibility: Suitable for aircraft metals, well-bonded paint, and painted or unpainted aircraft surfaces.
    • Aluminum appearance protection: Formulated to clean aluminum without staining or streaking under suitable process conditions.
    • Free-rinsing formulation: Readily soluble and stable in water mixtures for efficient rinsing after cleaning.
    • Immersion and ultrasonic use: Designed for dip tanks, immersion cleaning, and ultrasonic parts-cleaning systems.
    • Nonflammable concentrate: Supplied as a nonflammable liquid alkaline cleaner.

    Applications / Suitable for

    • Painted and unpainted aircraft exterior surfaces
    • Aircraft interior surfaces
    • Aircraft metals and well-bonded paint
    • Immersion and dip cleaning
    • Ultrasonic parts-cleaning tanks
    • Metal pretreatment processes
    Product Family

    BONDERITE C-AK 5948-R

    Catalog Product

    Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

    TDS, SDS & Technical Documents

    Technical Specifications

    Other Properties
    Storage TemperatureStorage Temperature
    0–40°C °C
    General Properties
    AppearanceAppearance
    Blue liquid
    Specific GravitySpecific Gravity
    1.01–1.02 g/cm³

    Additional Information

    Technical properties

    As-supplied / before-processing properties

    Supplier-published characteristics and storage information for BONDERITE® C-AK 5948 R EU AERO.

    Property Value Unit Method / condition
    Technology Metal pretreatment — Supplier classification
    Product type Alkaline cleaner — Supplier classification
    Application Immersion — Supplier classification
    Appearance Blue liquid — As supplied
    pH 11.7–12.3 — 100% product at 20°C; potentiometric method
    Density 1.01–1.02 g/mL At 20°C
    Kinematic viscosity 1–10 mm²/s At 20°C
    Water solubility Miscible — Qualitative, at 20°C
    Flash point >100 °C Product classified as nonflammable
    Storage temperature 0–40 °C Store cool and frost-free
    Shelf life 24 months In unopened original packaging
    Technical properties

    After-processing / operating properties

    Supplier-published operating and bath-control conditions for immersion cleaning with BONDERITE® C-AK 5948 R EU AERO.

    Property Value Unit Method / condition
    Working concentration 5–25 % v/v Diluted in water; selected according to soil level
    Operating temperature 65–80 °C Immersion cleaning
    Contact time 5–15 minutes Immersion cleaning
    Ultrasonic compatibility Suitable — Supplier identifies product as ideal for ultrasonic tanks
    Bath-control endpoint 5.2 pH Titrate 100 mL bath sample with 1.0 N sulfuric acid
    Bath concentration calculation V × 17.8 mL/L V = mL of 1.0 N H₂SO₄ used to reach pH 5.2

    Leading Brands Trust in Our Products and Services

    • Jabil
    • Linxens
    • Magna
    • Medtronic
    • NXP
    • Philips
    • Semikron
    • Teledyne
    • Thales
    • Vishay
    • ZF
    • AMS
    • Apple
    • Audi
    • Broadcom
    • Borgwarner
    • Bosch
    • Eaton
    • Henkel
    • Honeywell
    • Hysol
    • Intel
    Products that Perform|Knowledge that Serves|Service that Delivers