COOLTHERM UR388

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM UR388

Main features

  • 0.7 W/(m K) Thermal Encapsulation
  • 6,000 cP Mixed Viscosity
  • 0.32% TML and 0.02% CVCM

Product Description

CoolTherm® UR-388 FST Flame Retardant Urethane Encapsulant is a two-component urethane system for encapsulating and casting applications. It cures at room temperature to form a flame-retardant, semi-flexible material with typical thermal conductivity of 0.7 W/m·K and an operating-temperature range of -55°C to +130°C. The mixed system has a typical viscosity of 6,000 cP at 25°C and combines low cure exotherm with documented thermal-shock resistance and low-outgassing performance in high-vacuum test conditions. :contentReference[oaicite:0]{index=0}

Key features

  • Thermally conductive encapsulation: Provides typical cured thermal conductivity of 0.7 W/m·K.
  • Low-outgassing performance: Records 0.32% total mass loss and 0.02% collected volatile condensable materials under ASTM E595-77.
  • Room-temperature cure: Initially cures in less than 30 minutes at 25°C and may be mildly heat-cured at 60°C to accelerate cure.

Applications / Suitable for

  • Encapsulating applications
  • Casting applications
Product Family

COOLTHERM UR388

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Resin: Black Liquid | Hardener: Amber Liquid | Mixed: Black Liquid
Specific GravitySpecific Gravity
Resin: 1.53 | Hardener: 1.24 |
Physical Properties
Viscosity (Part A)Viscosity (Part A)
(Resin) 15000 mPa.s
Viscosity (Part B)Viscosity (Part B)
(Hardener) 70 mPa.s
Thermal Properties
Thermal ConductivityThermal Conductivity
0.7 W/m.K
Mechanical Properties
ElongationElongation
at break 50 %
Electrical Properties
Dielectric StrengthDielectric Strength
15 kV/mm
Volume ResistivityVolume Resistivity
7 x 10^15 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of CoolTherm UR-388 FST resin, UR-388 hardener and the mixed encapsulant before cure. Values are not intended for specification purposes. :contentReference[oaicite:1]{index=1}

Property Value Unit Method / condition
Appearance Black liquid / Amber liquid / Black liquid — UR-388 FST resin / UR-388 hardener / mixed system
Viscosity 15,000 / 70 / 6,000 cP Resin / hardener / mixed system at 25°C; test method not stated
Specific gravity 1.53 / 1.24 / 1.50 — Resin / hardener / mixed system; test conditions not stated
Mix ratio 100:20 / 100:24 Resin:hardener By weight / by volume
Gel time 5 minutes Mixed system at 25°C; test method not stated
Suggested cure schedule 24 hours to 7 days — At 25°C; initial cure occurs in less than 30 minutes
Shelf life 6 months Each component from date of manufacture when stored at 25°C in the original, unopened container
Technical properties

After-processing / final-state properties

Typical cured properties of CoolTherm UR-388 FST. The source does not identify the cure schedule used to prepare the cured-property specimens. Values are not intended for specification purposes. :contentReference[oaicite:2]{index=2}

Property Value Unit Method / condition
Thermal conductivity 0.7 W/m·K Test method, temperature and specimen thickness not stated
Operating-temperature range -55 to +130 °C Documented range for parts and devices; retained-property data are not stated
Hardness 88 Shore A ASTM D2240
Tensile strength 15.58 (2,260) MPa (psi) ASTM D638
Elongation at break 50 % ASTM D638
Volume resistivity 7 × 1015 ohm-cm At 25°C; ASTM D257
Dielectric constant 6.2 — At 25°C and 1 MHz; ASTM D150
Dissipation factor 0.013 — At 25°C and 1 MHz; ASTM D150
Total mass loss 0.32 % ASTM E595-77
Collected volatile condensable materials 0.02 % ASTM E595-77

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers