DOWSIL 92-009

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

DOWSIL 92-009

Main features

  • Room-Temperature Coating Cure
  • Brush, Dip, Pour, and Spray Application
  • Coating Build of 5 to 6 Mils

Product Description

DOWSIL™ 92-009 Dispersion Coating is a one-part, air-drying silicone coating formulated for environmental sealing and surface protection. Supplied as 35% silicone solids dispersed in a hydrocarbon solvent, it can be applied by brushing, dipping, pouring, or spraying and cures at room temperature to form a tough, transparent silicone rubber film. The cured coating combines high tear strength with adhesion, release, anti-abrasion, electrical-insulation, and environmental-resistance properties.

Key features

  • One-part room-temperature cure: Air-dries through exposure to atmospheric moisture and cures within 72 hours at 25°C (77°F) and 50% relative humidity.
  • Durable protective film: Cures to a tough, transparent silicone rubber coating with high tear strength and anti-abrasion characteristics.
  • Environmental resistance: Resists weathering, ozone, chemicals, moisture, ice, and ultraviolet radiation at temperatures up to 260°C (500°F).
  • Flexible application methods: May be applied by brushing, dipping, pouring, or spraying.

Applications / Suitable for

  • Environmental sealing and protection of parts and substrates
  • Protective coating for electrical and steel cables, structural members, and equipment components
  • Corrosion and erosion protection for aircraft, launch equipment, and related aerospace components
Product Family

DOWSIL 92-009

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
clear
Specific GravitySpecific Gravity
1.11
Thermal Properties
Flash PointFlash Point
18 °C
Physical Properties
Tack-Free TimeTack-Free Time
40 minutes
ViscosityViscosity
82 mPa.s
Mechanical Properties
ElongationElongation
680 %
Electrical Properties
Volume ResistivityVolume Resistivity
5.4 x 10^14 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied and processing properties. Values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Physical form 35% silicone solids dispersed in hydrocarbon solvent — As supplied
Color Translucent — CTM 0176
Flash point 18 (65) °C (°F) CTM 0021A
Viscosity 82 poise CTM 0050
Tack-free time 40 minutes CTM 0095
Average build per coat 5–6 mils Applied as supplied
Cure time 72 hours At 25°C (77°F) and 50% relative humidity
Shelf life 9 months From date of manufacture when stored below 30°C (86°F) in closed containers
Technical properties

After-processing / final-state properties

Typical cured-material properties. Values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Physical form Tough, transparent silicone rubber coating — After cure
Specific gravity 1.11 — CTM 0022
Adhesion to primed 2024 aluminum Excellent — 2024 aluminum; primed
Tensile strength 1,300 psi ASTM D 412; cured 72 hours at 25°C (77°F) and 50% relative humidity
Elongation 680 % ASTM D 412; cured 72 hours at 25°C (77°F) and 50% relative humidity
Tear strength, Die B 180 ppi ASTM D 624; cured 72 hours at 25°C (77°F) and 50% relative humidity
Durometer hardness 46 Shore A points ASTM D 676; cured 72 hours at 25°C (77°F) and 50% relative humidity
Volume resistivity 5.4 × 1014 ohm-cm CTM 0249; cured 72 hours at 25°C (77°F) and 50% relative humidity
Thermal conductivity 1.26 Btu-in/ft²·h·°F CTM 0224; cured 72 hours at 25°C (77°F) and 50% relative humidity

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers