DOWSIL SE 4445

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

DOWSIL SE4445

Main features

  • Two-Component Electronics Silicone System
  • White/Charcoal Component Identification
  • 2.4 Relative Density

Product Description

DOWSIL™ SE 4445 CV Gel is a two-component silicone compound identified for electrical and electronics applications. The supplied Part A is a white liquid with a typical relative density of 2.4 and dynamic viscosity of 80 poise, while Part B is a charcoal liquid with a typical relative density of 2.4 and dynamic viscosity of 230 poise. Product-specific thermal performance, mix ratio, cure schedule, cured hardness, working time, gap capability, and final-state properties cannot be published because the referenced technical data sheet was not included in the supplied files. :contentReference[oaicite:0]{index=0} :contentReference[oaicite:1]{index=1}

Key features

  • Two-component silicone system: Supplied as separate Part A and Part B silicone compounds.
  • Distinct component colors: Part A is white and Part B is charcoal, supporting visual differentiation during handling.
  • Electronics-focused use: Both component safety data sheets identify electrical industry and electronics use.

Applications / Suitable for

  • Electrical industry and electronics applications
Product Family

DOWSIL SE 4445

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
White/Black
Component SystemComponent System
Two Part
Mix RatioMix Ratio
1:1
Physical Properties
ViscosityViscosity
15025 mPa.s
Thermal Properties
Thermal ConductivityThermal Conductivity
1.3 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical physical properties reported in the supplied Part A and Part B safety data sheets. These values are not specifications. :contentReference[oaicite:2]{index=2} :contentReference[oaicite:3]{index=3}

Property Part A Part B Unit Method / condition
Physical state Liquid Liquid — As supplied
Color White Charcoal — As supplied
Relative density 2.4 2.4 — Water = 1; test temperature not stated
Dynamic viscosity 80 230 poise Test method, temperature and shear conditions not stated
Boiling point >100 >100 °C At 760 mmHg
Flash point >93.3 >100 °C Closed cup

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers