Bi58Sn42 | Eutectic Pbfree Solder Spheres

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

Bi58Sn42 Eutectic Leadfree Solder SpheresBi58Sn42 | Eutectic Pbfree Solder SpheresBi58Sn42 Eutectic Leadfree Solder Spheres

Main features

  • Leadfree Solder Spheres
  • Lowest Cost Eutectic (138°C) Solder
  • Low-Temperature Eutectic Solder

Product Description

LINQALLOY Bi58Sn42 Low-temperature eutectic solder spheres are lead-free Bismuth-Tin alloys that contain 58% Bismuth (Bi), 42% Tin (Sn) and are often written as 58Bi42Sn, Sn42Bi58, or 42Sn58Bi. Bi58Sn42 Solder Spheres are low-temperature, lead-free, eutectic solder spheres and are used by companies working with BGA, CSP, LBGA, PBGA and CBGA components who have made the transition to Lead-free (Pb-free) soldering.

Features:

  • Lowest Cost Eutectic (138°C) Solder
  • Low-Temperature Eutectic Solder compared to Tin-Silver
  • Compatible with many Flux Types
  • Lead-free

Each jar has a clear label on the lid specifying the solder ball diameter as well as a label on the front identifying the alloy type, the quantity of spheres in the jar, the date of manufacture, and the product lot (or batch) number. This batch number is also tied to a certificate of conformance that is provided with the solder spheres and ensures the Bi58Sn42 solder spheres meet the following quality criteria:

  • Tin (Sn): 42%
  • Bismuth (Bi): 58%
  • Eutectic Temperature: 138°C
  • Melting Temperature (Solidus): 138°C
  • Melting Temperature (Liquidus): 138°C
  • Sphericity: Within 1.5%

Diameter Tolerance

  • 0.1mm - 0.25mm (100µm - 250µm) : ± 0.0050mm (± 5µm)
  • 0.3mm - 0.45mm (300µm - 450µm) : ± 0.010mm (± 10µm)
  • 0.5mm - 0.89mm (500µm - 890µm) :  ± 0.020mm ( ± 20µm)
Product Family

LINQ Bi58Sn42

1. Select Diameter
2. Select Package Size
Price starting from €62.21
Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Please select Diameter and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy CompositionAlloy Composition
Bi58Sn42
Alloy TypeAlloy Type
Bi58Sn42
Specific GravitySpecific Gravity
8.56g/cc
Spheroid ToleranceSpheroid Tolerance
1.5 %
Other Properties
RoHS CompliantRoHS Compliant
Yes

Additional Information

The solder spheres you receive are originally manufactured solder spheres packed into jars with inert gas (nitrogen). We do not repack the solder balls, so the jars you will receive have never been opened, thus ensuring the quality of the product. The lid of the jar is also always sealed with a shrink-wrapped plastic wrap ensuring that the solder spheres do not oxidate in the jar.

Presentation

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers