PIT1A-ESD-BRL | 1 mil Black Conductive ESD Tape with Acrylic Adhesive & Release liner

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

PIT1A-ESD-BRL | 1 mil Black Conductive ESD Tape with Acrylic Adhesive & Release liner

Main features

  • 1 mil polyimide film
  • Acrylic adhesive with release liner
  • >6500V breakdown voltage

Product Description

LINQTAPE PIT1A-ESD-BRL is a high-temperature resistant, antistatic-treated polyimide tape with an electro-static discharge designed for both permanent and temporary bonding in many high-temperature applications. With an acrylic adhesive, this tape has the same mechanical properties as our standard PIT1A-Series products but is black and has a 1µm conductive polymer that provides electro-static discharge and makes the tape anti-static.

LINQTAPE PIT1A-ESD-BRL tapes get their conductivity by being carbon-loaded. As such the film provides both thermal conductivity as well as antistatic control with a surface resistance of less than 10E9 ohms per square. This product is an alternative to Kapton XC film with an acrylic adhesive layer. This version comes with a release liner, ensuring that the adhesive won't dry. The non-release liner product has been discontinued. Please contact us for more widths.

 

Key Features:

  • Excellent insulating properties
  • Carbon-loaded conductivity
  • Designed for permanent and temporary bonding
  • Acrylic adhesive
Product Family

LINQ PIT1A-ESD-BRL

1. Select Width
2. Select Length
Price starting from €495.62
Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive LayerAdhesive Layer
Acrylic
Adhesive ThicknessAdhesive Thickness
38.1 µm
Chemistry TypeChemistry Type
Polyimide
ColorColor
Black
Film ThicknessFilm Thickness
25.4 µm
Release LinerRelease Liner
Yes
Single or Double-Sided AdhesiveSingle or Double-Sided Adhesive
Single
Special LayerSpecial Layer
Antistatic Polymer coating
Total ThicknessTotal Thickness
63.5 μm
Thermal Properties
Temperature ResistanceTemperature Resistance
155 ˚C
Electrical Properties
Breakdown VoltageBreakdown Voltage
6500 V
Dielectric StrengthDielectric Strength
256 kV/mm
Other Properties
RoHS CompliantRoHS Compliant
Yes
VOC-Free (100% solids content)VOC-Free (100% solids content)
Yes
Mechanical Properties
Adhesion StrengthAdhesion Strength
25 Oz/in
ElongationElongation
55 %
Tensile Strength (Thin Film)Tensile Strength (Thin Film)
54 N/cm

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers