Loctite E-30CL EPOXY ADHESIVE

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite E-30CL EPOXY ADHESIVE

Main features

  • Minimally Shrinking Epoxy Bondline
  • Two-Part Ambient-Cure Processing
  • Adhesion to Glass

Product Description

LOCTITE® EA E-30CL™ Epoxy Adhesive is a low-viscosity, two-component industrial epoxy for bonding, small potting, staking, and laminating applications. The resin and amine hardener mix at a 2:1 ratio by volume and cure at room temperature with minimal shrinkage to form an ultra-clear, colorless-to-slightly-yellow bondline. The cured material combines structural and electrical insulating properties with resistance to a range of chemicals and solvents. Documented bonding substrates include glass, optical fibers, ceramics, metals, and many rigid plastics.

Key features

  • Ultra-clear cured bondline: Cures with minimal shrinkage to a colorless-to-slightly-yellow solid for applications where optical clarity is required.
  • Low-viscosity, self-leveling processing: The mixed adhesive is free-flowing and self-leveling, with a 30-minute working time at 25°C.
  • Structural and electrical performance: The cured epoxy provides a typical tensile strength of 55 N/mm² and dielectric breakdown strength of 20 kV/mm.

Applications / Suitable for

  • Bonding applications requiring optical clarity
  • Small potting applications
  • Component staking
  • Laminating applications
  • Bonding glass, optical fibers, ceramics, metals, and many rigid plastics
Product Family

LOCTITE E-30CL

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Clear to slight yellow
Chemistry TypeChemistry Type
Resin - Epoxy, Hardener - Amine
Component SystemComponent System
two component
Mix RatioMix Ratio
2:1
Pot LifePot Life
30 minutes
Specific GravitySpecific Gravity
1.07
Physical Properties
Tack-Free TimeTack-Free Time
160 minutes

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the resin, hardener, and mixed adhesive before cure. Values are not intended for preparing specifications.

Property Value Unit Method / condition
Components Two — Epoxy resin and amine hardener; requires mixing
Appearance Clear, colorless to slightly yellowish liquid — Resin and hardener
Mix ratio by volume 2:1 — Resin:hardener
Mix ratio by weight 100:46 — Resin:hardener
Resin viscosity 10,500 mPa·s (cP) Brookfield RVT, spindle 6, 20 rpm, 25°C
Hardener viscosity 2,250 mPa·s (cP) Brookfield RVT, spindle 5, 20 rpm, 25°C
Mixed specific gravity 1.07 — At 25°C
Working time 30 minutes At 25°C after mixing
Technical properties

After-processing / final-state properties

Typical properties of the cured adhesive. Bulk properties were measured after curing for 5 days at 25°C; adhesive-strength conditions are identified separately. Values are not intended for preparing specifications.

Property Value Unit Method / condition
Appearance Colorless to slightly yellowish solid — Mixed and cured material
Shore hardness 80–90 Shore D ISO 868; cured 5 days at 25°C
Glass transition temperature 61 °C ASTM E1640; cured 5 days at 25°C
Tensile strength 55 (8,000) N/mm² (psi) ISO 527-2; cured 5 days at 25°C
Elongation 8 % ISO 527-2; cured 5 days at 25°C
Dielectric breakdown strength 20 kV/mm IEC 60243-1; cured 5 days at 25°C
Lap shear strength on grit-blasted steel 21 (3,100) N/mm² (psi) Cured 5 days at 22°C
Block shear strength on glass 24 (3,540) N/mm² (psi) ISO 13445; cured 5 days at 22°C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers