LOCTITE EA 9321

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA 9321

Main features

  • Thixotropic Application Control
  • Room-Temperature Retention Cure
  • 1,000 psi Lap Shear

Product Description

LOCTITE® EA 9321 AERO is a two-component, thixotropic epoxy paste adhesive for aerospace potting, edge-fill and structural bonding applications. The gray adhesive cures at room temperature and can also be heat cured when a faster process is required. It forms tough, durable bonds and retains useful strength across a broad test-temperature range, with a defined service temperature of approximately 250°F (121°C) based on 1,000 psi (6.9 MPa) lap shear strength. Its paste consistency supports controlled application, while a 40-minute pot life at 77°F (25°C) provides time for mixing, dispensing and assembly.

Key features

  • Dual-cure capability: Cures in 5–7 days at 77°F (25°C), with an alternative complete cure of 1 hour at 180°F (82°C).
  • Elevated-temperature strength: Provides an approximate service temperature of 250°F (121°C), defined at 1,000 psi (6.9 MPa) lap shear strength.
  • Thixotropic paste consistency: Supports controlled placement in potting, edge-fill and structural bonding applications.

Applications / Suitable for

  • Aerospace potting
  • Edge-fill applications
  • Structural bonding
  • OEM and maintenance, repair and overhaul applications

Technical Specifications

General Properties
ColorColor
Gray (Part A) / Off white (Part B) / Gray (Mixed)
DensityDensity
1240 / 1220 kg/m3
Physical Properties
Viscosity (Part B)Viscosity (Part B)
20000–80000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component and mixed-material properties. Keep Part A, Part B and mixed-material values distinct during product evaluation and processing.

Property Value Unit Method / condition
Color Part A: Gray
Part B: Off white
Mixed: Gray
— Uncured components and mixed adhesive
Viscosity — Part A 2,900–7,100 Poise 77°F; Brookfield HBT, spindle 7 at 20 rpm
Viscosity — Part B 200–800 Poise 77°F; Brookfield HBT, spindle 5 at 20 rpm
Density Part A: 1.24
Part B: 1.22
Mixed: 1.23
g/ml Uncured components and mixed adhesive
Mix ratio by weight 100:50 Parts by weight Part A:Part B; volume measurement is not recommended for structural applications without ratio-control precautions
Pot life 40 minutes 450 g mixed mass at 77°F (25°C); ASTM D2471, water bath
Shelf life at ≤77°F (25°C) Part A: 3 months
Part B: 1 year
— Store in the intended conditions after receipt

After-processing / final-state properties

Typical cured-material and bonded-joint properties. Values depend on the stated cure, specimen, substrate, preparation and test conditions.

Property Value Unit Method / condition
Tensile lap shear strength 4,000 psi ASTM D1002 at 77°F (25°C); 2024-T3 AlClad aluminum, FPL etched; 7 days at 77°F (25°C) or 1 hour at 180°F (82°C)
Service temperature Approximately 250 °F 121°C; defined where ASTM D1002 lap shear strength remains 1,000 psi (6.9 MPa)
Tensile strength 7,100 psi ASTM D638; 0.125 in (3.18 mm) casting at 77°F (25°C)
Tensile modulus 420 ksi ASTM D638; 0.125 in (3.18 mm) casting at 77°F (25°C)
Elongation at break 6 % ASTM D638; 0.125 in (3.18 mm) casting at 77°F (25°C)
Hardness 84 Shore D Cured bulk resin at 77°F (25°C)
Glass-transition temperature Dry: 230
Wet: 190
°F Dry: 110°C; wet: 88°C
Compressive strength Yield: 9,280
Ultimate: 16,880
psi ASTM D695; 0.5 in (12.7 mm) casting at 77°F (25°C)

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers