LOCTITE EC210

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

LOCTITE EC210

Main features

  • General-Purpose Electrical Insulation Coating
  • 55:35 Two-Part Mixing
  • 55 to 150 deg C Service Range

Product Description

ECCOCOAT® EC210 A/B is a general-purpose, oxide-filled epoxy surface coating formulated for protecting electrical, electronic, and industrial components from moisture, chemicals, and environmental exposure. This two-component, solvent-containing epoxy coating provides excellent adhesion to metals, plastics, wood, glass, ceramics, concrete, and masonry surfaces. Once cured, it delivers durable mechanical performance, excellent electrical insulation properties, and long-term weather resistance for coating and encapsulation applications.

Key Features & Benefits

  • General-purpose oxide-filled epoxy coating system.
  • Excellent resistance to moisture, chemicals and weathering.
  • Outstanding adhesion to a wide range of substrates.
  • Excellent electrical insulation properties.
  • Suitable for brush or spray application.
  • Reliable protection for electronic assemblies.
  • Wide operating temperature capability.

Recommended Applications

  • Electrical and electronic component coating.
  • Circuit and equipment protection.
  • Concrete, brick and masonry coating.
  • Metal, wood and plastic surface protection.
  • General industrial environmental protection coatings.
Product Family

LOCTITE EC210

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Technical Specifications

No specifications available.

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Chemical Type (Part A) Epoxy — Oxide-filled coating resin
Chemical Type (Part B) Solvent Containing Amine — Hardener
Appearance (Part A) Opaque Liquid — Visual
Appearance (Part B) Clear Liquid — Visual
Density (Part A) 1.70 g/cm³ ASTM D792
Density (Part B) 0.98 g/cm³ ASTM D792
Mix Ratio (Weight) 35 parts B / 100 parts A By weight
Mix Ratio (Volume) 55 parts B / 100 parts A By volume
Working Life 4 hours 100 g @ 25°C
Mixed Viscosity 1,000 cP ASTM D2393
Mixed Density 1.40 g/cm³ ASTM D792
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Hardness 88 Shore D ASTM D2240
Operating Temperature Range -55 to +150 °C Continuous service
Dielectric Strength 16.5 kV/mm ASTM D149
Dielectric Strength 420 V/mil ASTM D149
Dielectric Constant 4.6 — 60 Hz, ASTM D150
Dissipation Factor 0.02 — 60 Hz, ASTM D150
Volume Resistivity 1 × 10¹³ Ohm-cm 25°C, ASTM D257
Cure Schedule 24 hours 25°C cure
Accelerated Cure Schedule 1 hour 77°C cure
Recommended Post Cure 2 - 4 hours At highest expected use temperature

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers