Product Description

LOCTITE® LB 8150™ is a high-temperature anti-seize lubricant formulated with mineral oil, lithium soap, graphite, aluminum and extreme-pressure additives to protect threaded assemblies exposed to severe thermal conditions. The non-curing compound prevents seizure, galling, corrosion, and jamming of threaded components operating at temperatures up to 900°C. It is particularly suitable for exhaust systems, burners, and industrial equipment where reliable assembly and future disassembly are required.

Key Features & Benefits

  • High-temperature anti-seize formulation.
  • Protects threaded connections from seizing and corrosion.
  • Contains graphite and aluminum lubricating solids.
  • Extreme pressure additive technology.
  • Suitable for service temperatures up to 900°C.
  • Prevents jamming in high-temperature assemblies.
  • Tested to MIL-PRF-907-H requirements.

Recommended Applications

  • Exhaust systems of combustion engines.
  • Oil and gas burner fittings.
  • High-temperature threaded fasteners.
  • Industrial furnace and thermal processing equipment.
  • Maintenance applications requiring future disassembly.
Product Family

LOCTITE LB8150

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Grey
Density (g)Density (g)
0.9 g/cm3

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Anti-Seize — Non-curing lubricant
Chemical Type Mineral Oil, Lithium Soap, Graphite, Aluminum & EP Additives — High temperature formula
Appearance Grey — As supplied
Density 0.9 g/mL ISO 2811-1 @ 25°C
NLGI Consistency 1 Class ISO 6743-99
Worked Penetration 310 - 340 0.1 mm ISO 2137, 60 strokes @ 25°C
MIL Specification MIL-PRF-907-H — Tested to specification requirements
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Operating Temperature Range -30 to +900 °C Typical service range
Peak Temperature 900 °C Maximum rated temperature
4-Ball Weld Load 4,400 N ASTM D2596
Weld Scar Diameter <4.0 mm ASTM D2596 @ 4,400 N
Wear Scar 0.95 mm 1 hour / 400 N test
Copper Corrosion 1b Rating ISO 2160, 3 h @ 100°C
Seizure Prevention Excellent — High-temperature threaded assemblies
Corrosion Protection Excellent — Prevents thread seizure and galling

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers