LOCTITE LB8700

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LOCTITE LB8700

Main features

  • Molybdenum Disulfide Anti-Seize Formulation
  • Galling Prevention in Assembly
  • Improved Clamp Load Consistency

Product Description

LOCTITE® LB 8700™ (Moly 50™) is a molybdenum disulfide-based anti-seize and thread lubricant designed to prevent galling, seizure, and wear in threaded fasteners and metal assemblies. The non-curing compound provides excellent lubricity, improves clamp load consistency, and facilitates future disassembly of components exposed to elevated temperatures and demanding service conditions. It is suitable for machine threads, tapered pipe threads, press-fit joints, and slip-fit assemblies.

Key Features & Benefits

  • Molybdenum disulfide anti-seize formulation.
  • Prevents galling and seizing of threaded components.
  • Improves clamp load consistency.
  • Provides excellent lubricity under load.
  • Suitable for press-fit and slip-fit joints.
  • Non-curing paste for easy assembly and disassembly.
  • Tested to MIL-PRF-83483 requirements.

Recommended Applications

  • Machine threads and fasteners.
  • Tapered pipe threads.
  • Press-fit assemblies.
  • Slip-fit joints.
  • Industrial maintenance and assembly operations.
Product Family

LOCTITE LB8700

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Smooth gray colored paste
Specific GravitySpecific Gravity
1.41

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Molybdenum Disulfide Based — Anti-seize lubricant
Appearance Smooth Gray Paste — Single-component
Specific Gravity 1.41 — 25°C
Penetration 170 - 260 0.1 mm ISO 2137
Weight per Gallon 10.99 - 11.99 lb/gal Typical
MIL Specification MIL-PRF-83483 — Qualified test requirements
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Operating Temperature Range -29 to +398 °C Typical service range
Torque Coefficient (K Factor) 0.13 — Lubricated 12.7 mm grade 8 bolt
Torque Coefficient (Unlubricated) 0.27 — Solvent-cleaned fastener
Clamp Load Efficiency Improved — Higher preload at equivalent torque
Thread Lubrication Excellent — Machine and pipe threads
Press-Fit Compatibility Suitable — Assembly and disassembly aid
Slip-Fit Compatibility Suitable — Surface protection and lubrication
Seizure Protection Excellent — High-load threaded assemblies

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers