LORD 606/6

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

LORD 606/6

Main features

  • Difficult Dcpd-Based FRP Bonding
  • 4 to 6-Minute Working Window
  • Glass-Bead Bondline Control

Product Description

LORD® 606 Acrylic Adhesive with LORD® Accelerator 6GB is a fast-setting, two-component structural acrylic adhesive system designed for bonding difficult composite substrates, including DCPD and modified DCPD resin-based fiber-reinforced plastics. The mixed adhesive can also cross-bond composites to supported metals and plastics while providing strong bonds, good surface cure and minimal surface preparation. Glass beads in LORD® Accelerator 6GB help control the adhesive bondline thickness.

Key Features

  • Composite bonding capability for DCPD-based FRP and cross-bonding composites to supported metals and plastics.
  • Fast room-temperature processing with a 4–6 minute working time and handling strength in 16–24 minutes at 75°F (24°C).
  • Controlled bondline thickness through the glass-bead content of LORD® Accelerator 6GB.
  • Non-sag application allows placement on vertical and overhead surfaces.

Applications / Suitable for

  • DCPD and modified DCPD resin-based FRP bonding
  • FRP-to-FRP structural bonding
  • Composite-to-metal cross-bonding
  • Composite-to-plastic cross-bonding
Product Family

LORD 606/6

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
White to Off-white Paste
DensityDensity
1042 -1162 kg/m3
Physical Properties
ViscosityViscosity
100,000 - 300,000 mPa.s
Thermal Properties
Flash PointFlash Point
15 °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Typical properties of LORD® 606 Acrylic Adhesive and the mixed system with LORD® Accelerator 6GB. Values are typical and are not intended for specification purposes.

Property Value Unit Method / Condition
Appearance White to off-white paste — LORD 606 adhesive, typical
Viscosity 100,000–300,000 cP Typical
Density 8.7–9.7
(1042–1162)
lb/gal
(kg/m³)
LORD 606 adhesive, typical
Flash Point 59
(15)
°F
(°C)
Typical
Mix Ratio 7.3:1
10:1
by weight
by volume
LORD 606 adhesive to LORD Accelerator 6GB
Solids Content 100 % Mixed adhesive system
Working Time 4–6 minutes At 75°F (24°C)
Time to Handling Strength 16–24 minutes At 75°F (24°C); time to develop 100 psi
Mixed Appearance Grey paste — With LORD Accelerator 6GB
Shelf Life 6 months Store below 80°F (27°C) in the original, unopened container; 40–50°F (4–10°C) recommended
Technical Properties

After-Processing / Final-State Properties

Typical cured properties and supported bond-performance data for LORD® 606 Acrylic Adhesive with LORD® Accelerator 6GB. Values are typical and are not intended for specification purposes.

Property Value Unit Method / Condition
Complete Cure Time 8–24 hours Depends on temperature and bondline thickness
Cured Appearance White to grey — Tack-free surface
Elongation 12 % ASTM D882-83A, modified
Glass Transition Temperature (Tg) 225
(107)
°F
(°C)
ASTM E1640-99, by DMA
Aluminum-to-Aluminum Lap Shear 2776
(19.1)
psi
(MPa)
Room temperature; IPA-wiped aluminum; 0.010 in film; 24-hour room-temperature cure; 10:1 by volume
Galvanized-Steel Lap Shear 2063
(14.2)
psi
(MPa)
Room temperature; 0.010 in film; 24-hour room-temperature cure; 10:1 by volume
ABS-to-ABS Lap Shear 595
(4.1)
psi
(MPa)
Room temperature; 24-hour room-temperature cure; 10:1 by volume; stock-break failure
FRP-to-FRP Lap Shear 1106
(7.6)
psi
(MPa)
Room temperature; dry-rag-wiped FRP; 0.030 in film; 24-hour room-temperature cure; fiber-tear failure
FRP-to-ABS Lap Shear 440
(3.0)
psi
(MPa)
Room temperature; 24-hour room-temperature cure; stock-break failure

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers