MOLYKOTE 33

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE 33MOLYKOTE 33

Main features

  • NLGI 2 Silicone Grease
  • Water-Resistant Light-Load Lubrication
  • 73 to 180 deg C Service Range

Product Description

MOLYKOTE® 33 Medium Extreme Low Temperature Grease is a white, approximately NLGI 2 silicone-oil grease thickened with lithium soap for light-load metal-to-metal and metal-to-plastic contacts operating from low to high speeds. Its documented service range is -73°C to 180°C, with low-temperature torque values measured at -73°C. The grease is water-resistant and has documented oxidation, bleed, evaporation, oil-separation, and four-ball weld-load data for technical evaluation. Applications include roller and conveyor equipment, control cables, electric motors, precision optical and measurement equipment, and refrigerators or freezers. Apply to clean lubrication points by brush, spatula, or automatic lubrication equipment, and verify compatibility with the specific plastic, elastomer, and existing lubricant in the intended assembly.

Key features

  • Extreme low-temperature service range: Documented for use from -73°C to 180°C in light-load lubrication applications.
  • Silicone grease system: Silicone oil thickened with lithium soap, with approximately NLGI 2 consistency and no solid lubricants.
  • Measured torque at -73°C: ASTM D1478-80 results of 207 × 10-3 N·m initial breakaway torque and 32 × 10-3 N·m after 20 minutes.
  • Retention and aging data: Typical bleed, evaporation, oil-separation, and oxidation-pressure-loss values support condition-specific evaluation.
  • Material and application flexibility: Water-resistant and described as compatible with most plastics; confirm the exact material grade and lubricant combination before use.

Applications / Suitable for

  • Roller and conveyor equipment
  • Rolling-element bearings, plain bearings, bushings, and sleeves
  • Control cables, power screw drives, slides, guides, and tracks
  • Electric motors and other light-load electrical mechanisms
  • Photographic, optical, measurement, refrigerator, and freezer equipment
Product Family

MOLYKOTE 33

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Extreme low-temperature lubricating grease

MOLYKOTE® 33 Medium Extreme Low Temperature Grease

A white, lithium-thickened silicone grease for light-load metal-to-metal and metal-to-plastic contacts operating at low to high speeds. Its documented service range extends from -73°C to 180°C, with measured torque behavior at the low-temperature limit and supporting oxidation, bleed, evaporation, oil-separation, and four-ball weld-load data for application evaluation.

Approximately NLGI 2 -73°C to 180°C Silicone oil / lithium soap 76 cSt base oil at 40°C Water-resistant
MOLYKOTE 33 Medium Extreme Low Temperature Grease

MOLYKOTE® 33 Medium is supplied as a white, approximately NLGI 2 silicone grease.

As-supplied grease properties

Lubricant system
Silicone oil / lithium soap
Approximately NLGI 2 grease with no solid lubricants.
Consistency and base oil
260–300 mm/10
ISO 2137 worked penetration; base-oil viscosity is reported at both 25°C and 40°C.
Property Value Unit Method / condition
Color White — As supplied
Base oil / thickener Silicone oil / lithium soap — Product composition
Solid lubricants None — Product details
Kinematic base-oil viscosity 100 mm2/s DIN 51 562 at 25°C
Base-oil viscosity 76 cSt At 40°C
Worked penetration 260–300 mm/10 ISO 2137
NLGI class Approx. 2 — Consistency class
Density 0.98 g/cm3 ISO 2811 at 25°C

Typical values are not specification limits. Viscosity values measured at different temperatures are presented separately and should not be treated as equivalent.

Low-temperature and service performance

Service temperature range
-73°C to 180°C
The stated range defines supplier-recommended service limits; it does not imply unchanged consistency, friction, wear, or service life across the full range.
Torque at -73°C
207 / 32 × 10-3 N·m
ASTM D1478-80 initial breakaway torque and torque after 20 minutes of running, respectively.
Property Value Unit Method / condition
Service temperature range -73 to 180 °C Documented service range
Initial breakaway torque 207 × 10-3 N·m ASTM D1478-80 at -73°C
Torque after 20 min running 32 × 10-3 N·m ASTM D1478-80 at -73°C
Bleed ≤ 4.5 % ASTM D6184 at 150°C for 24 h
Evaporation ≤ 3.5 % ASTM D6184 at 150°C for 24 h
Oil separation 0.9 % DIN 51817 at 40°C for 7 days
Oxidation pressure loss 100 mbar DIN 51808; 100 h at 99°C
Four-ball weld load 1,400 N DIN 51350 pt. 4; 1,500 rpm for 1 min
Maximum Dn value 200,000 mm/min Screening value; bearing geometry not stated

Typical laboratory values are not guaranteed specifications. The four-ball weld load and maximum Dn value are selection inputs, not universal equipment load or speed ratings, and they do not establish a relubrication interval.

Application

Clean the lubrication point and apply with conventional grease methods

For light-load metal-to-metal or metal-to-plastic contacts, start with clean application points and select a method suited to the component geometry and grease-delivery system.

Surface preparation: Clean the points of application before adding grease.
Application methods: Apply or fill by brush, spatula, or automatic lubrication device.
Compatibility check: Confirm the specific plastic or elastomer grade and compatibility with any existing lubricant; broad material-family compatibility and NLGI grade do not establish mixture suitability.
 
Storage and Handling

Store in the original unopened container between 0°C and 40°C. Usable life is 60 months from the date of production under these conditions. Review the current safety data sheet and container label before handling.

Applications

Lubrication applications

Use contexts span light-load rolling, sliding, cable, and precision mechanisms. Product fit remains dependent on the specific materials, load, speed, temperature, lubricant quantity, and maintenance practice.

Roller or conveyor assembly with visible rolling-element bearings
Rollers, conveyors, and rolling bearings
Applications include roller and conveyor equipment and rolling-element bearings. Evaluate the grease for light-load contacts where low-temperature startup, speed, and lubricant delivery are important selection inputs.
guided sliding mechanism with a small lubricated contact area.
Control cables and guided motion
Use contexts include control cables, power screw drives, plain bearings, bushings, sleeves, slides, guides, and tracks. Match grease consistency and the application method to the mechanism and delivery system.
a refrigerator or freezer mechanism
Precision and cold-environment equipment
Applications include electric motors, photographic, optical, and measurement equipment, together with refrigerators and freezer equipment. For plastic or rubber/elastomer contacts, verify the exact material grade and exposure conditions.
Video resource

Rolling-element demonstration

This supplier-hosted video presents MOLYKOTE® 33 Medium in a rolling-element demonstration. Use it as a visual introduction to the product’s low-temperature positioning; final selection should remain based on the light-load scope, service conditions, contact materials, and equipment-specific evaluation.
Next steps

Evaluate MOLYKOTE® 33 Medium for your low-temperature lubrication application

Krayden can help review contact materials, load, speed, temperature, application method, lubricant compatibility, and grease-delivery requirements for bearings, cables, slides, precision mechanisms, and cold-environment equipment. Contact us to discuss product fit, sampling, or an application-specific evaluation plan.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers