MOLYKOTE EM-30L

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE EM-30L

Main features

  • -45 to 150 deg C Service Range
  • 3,730 N Four-Ball Weld Load
  • 0.4% Evaporation at 99 deg C

Product Description

MOLYKOTE® EM-30L Grease is a white, NLGI 1 polyalphaolefin grease thickened with lithium soap and formulated with PTFE and other solid lubricants for plastic-component mechanisms. It is intended for plastic/plastic, plastic/metal, and metal/metal interfaces in automotive, electrical, precision, audio, and office equipment. The documented service range is -45°C to 150°C, with low-temperature torque measured at -40°C. Typical test data include a 3,730 N four-ball weld load, a 0.5 mm four-ball wear scar, 0.4% evaporation at 99°C for 22 hours, and 5.0% bleed at 100°C for 24 hours. The silicone-free formulation is relevant where silicone contamination is a concern; confirm compatibility with the exact polymer, elastomer, coating, and existing lubricant before use.

Key features

  • Plastic-component grease system: NLGI 1 PAO grease with lithium-soap thickener, PTFE, and other solid lubricants.
  • Documented service range: -45°C to 150°C for product-selection evaluation.
  • Multiple contact pairings: Intended for plastic/plastic, plastic/metal, and metal/metal interfaces; confirm the exact material grade before use.
  • Load and wear data: Typical 3,730 N ASTM D2596 four-ball weld load and 0.5 mm ASTM D2266 wear scar under the stated test conditions.
  • Low-temperature torque data: Typical starting torque of 110 mN·m and running torque of 51 mN·m at -40°C.
  • Cleanliness-oriented formulation: White, silicone-free grease with documented low evaporation and supplier-described low seepage.

Applications / Suitable for

  • Automotive plastic parts and mechanisms
  • Electrical appliances with plastic components
  • Precision and audio equipment
  • Office-equipment plastic assemblies
  • Plastic-lubrication evaluation in gears, gearboxes, and pumps
Product Family

MOLYKOTE EM-30L

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Synthetic grease for plastic components

MOLYKOTE® EM-30L Grease

A white, silicone-free NLGI 1 grease based on polyalphaolefin oil, lithium soap, PTFE, and other solid lubricants. It is used for plastic/plastic, plastic/metal, and metal/metal contacts in automotive, electrical, precision, audio, and office equipment where low-temperature operation and controlled lubricant migration are relevant selection factors.

NLGI 1 PAO / lithium soap 90 mm²/s at 40°C -45°C to 150°C White, silicone-free
Approved product image showing MOLYKOTE EM-30L Grease packaging and label.

MOLYKOTE® EM-30L is a white PAO grease developed for plastic-component lubrication.

As-supplied grease properties

Lubricant system
PAO / lithium / PTFE
Polyalphaolefin base oil with lithium-soap thickener, PTFE, and other solid lubricants.
Consistency
NLGI 1
JIS K 2220 worked penetration of 325 after 60 strokes.
Base-oil viscosity
90 mm²/s
Typical kinematic viscosity at 40°C.
Property Value Unit Method / condition
Appearance White — As supplied
Base-oil viscosity 90 mm²/s At 40°C
Worked penetration 325 0.1 mm JIS K 2220; 60 strokes
Consistency class 1 NLGI Based on worked penetration
Density 0.91 g/cm³ Typical value

Typical values are not specification limits. Confirm current product data before establishing design or purchasing requirements.

Operating performance and test results

Use the documented operating range and condition-specific bench results as product-selection inputs. They do not establish universal equipment load capacity, wear life, material compatibility, or maintenance intervals.

Four-ball weld load
3,730 N
Typical ASTM D2596 result at 1,500 rpm for 1 minute.
Wear scar
0.5 mm
Typical ASTM D2266 result at 1,200 rpm, 392 N, for 1 hour.
Torque at -40°C
110 / 51 mN·m
Typical JIS K 2220 starting and running torque values.
Property Value Unit Method / condition
Service-temperature range -45 to 150 °C Supplier-documented operating range
Drop point 195 °C JIS K 2220
Bleed 5.0 % JIS K 2220; 100°C for 24 h
Evaporation 0.4 % JIS K 2220; 99°C for 22 h
Oxidation resistance 0.02 MPa JIS K 2220; 99°C for 100 h
Copper corrosion 1A rating JIS K 2220; 100°C for 24 h
Four-ball weld load 3,730 N ASTM D2596; 1,500 rpm for 1 min
Four-ball wear scar 0.5 mm ASTM D2266; 1,200 rpm, 392 N, 1 h
Low-temperature starting torque 110 mN·m JIS K 2220; -40°C
Low-temperature running torque 51 mN·m JIS K 2220; -40°C

Results are tied to the stated methods and conditions. Evaluate the grease in the intended component, material pairing, load, speed, temperature, and duty cycle before specification.

Application process

Prepare the interface and apply a controlled grease quantity

Application should match the component geometry and lubrication method. Material compatibility and lubricant-changeover conditions should be confirmed for the actual assembly.

Clean: Clean the points of application before introducing the grease.
Apply or fill: Use a brush, spatula, or automatic lubrication device according to the mechanism and production process.
Validate materials: Confirm the exact plastic, elastomer, coating, and any residual lubricant because compatibility can vary by grade, additives, stress, temperature, and exposure time.
Confirm the duty: Evaluate torque, load, wear, migration, and temperature behavior in the actual component before defining production fill or service practice.
Technician applying white grease in a controlled quantity to a clean plastic gear or plastic-to-metal mechanism.

Use clean application points and a controlled method suited to the component geometry.

Storage and Handling

Store unopened in a cool, dark place. Usable life is 36 months from the date of production. Keep the product in properly labeled containers, avoid strong oxidizing agents, and review the current safety data and container label before handling.

Applications

Plastic-component lubrication applications

The documented application scope includes automotive, electrical, precision, audio, and office equipment with plastic parts. Product fit remains specific to the polymer grade, contact pairing, component stress, speed, temperature, lubricant quantity, and contamination constraints.

Plastic gears and representative plastic mechanisms in an automotive assembly.
Automotive plastic mechanisms
For automotive parts using plastic/plastic or plastic/metal interfaces, the NLGI 1 consistency, -45°C low-temperature limit, and torque data are relevant selection inputs. Confirm the exact polymer grade, contact stress, speed, and exposure conditions.
Plastic gears and sliding contacts inside an electrical or audio equipment assembly.
Electrical and audio equipment
Electrical appliances and audio equipment are documented use contexts. The white, silicone-free formulation and supplier-described low seepage may be relevant where cleanliness and contact contamination require attention.
Precision or office equipment mechanism containing plastic-to-plastic and plastic-to-metal contacts.
Precision and office equipment
Precision and office mechanisms can include low-load gears, guides, and actuators with plastic interfaces. Evaluate starting torque, migration, wear, material compatibility, and the required production fill in the actual design.
Next steps

Evaluate MOLYKOTE® EM-30L for your plastic-component mechanism

Krayden can help review polymer and elastomer grades, plastic-to-plastic or plastic-to-metal interfaces, operating temperature, starting torque, load and wear requirements, lubricant migration, existing-lubricant compatibility, application method, and production fill strategy.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers