MOLYKOTE PA-744

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

MOLYKOTE PA-744

Main features

  • 10 to 20 um Screen-Printed Film
  • High-Wear High-Load Dry Lubrication
  • -75 to 300 deg C Service Range

Product Description

MOLYKOTE® PA-744 Anti-Friction Coating is a charcoal-gray, heat-cured dry-film lubricant containing graphite and molybdenum disulfide in an organic resin-solvent system. Formulated for screen-print application, it creates a long-term lubricating film for pistons used in automotive air-conditioning compressors, gasoline and diesel engines, pumps, and pneumatic or hydraulic systems. A recommended cured film thickness of 10–20 µm supports controlled coating application. The cured coating operates from −75°C to 300°C and provides high wear resistance, load-carrying capability, and resistance to motor oils under the documented conditions.

Key features

  • Screen-print application: Formulated for controlled deposition by screen printing.
  • Thin cured film: Recommended cured coating thickness is 10–20 µm.
  • Wide operating-temperature range: The cured coating operates from −75°C to 300°C.
  • Wear and load protection: Provides an extreme-wear-resistant coating with high load-carrying capacity.
  • Motor-oil resistance: Offers documented resistance to motor oils.
  • Run-in lubrication: Helps reduce piston and cylinder-wall wear during initial run-in and cold-start conditions.

Applications / Suitable for

  • Automotive air-conditioning compressor pistons
  • Gasoline and diesel engine pistons
  • Pistons used in pumps
  • Pneumatic-system pistons
  • Hydraulic-system pistons
  • Metal components requiring screen-printed dry-film lubrication
Product Family

MOLYKOTE PA-744

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product TypeProduct Type
Heat-cured anti-friction coating / dry-film lubricant
Specific GravitySpecific Gravity
1.21 g/mL at 25°C
Thermal Properties
Operating TemperatureOperating Temperature
−75°C to 300°C after cure °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied characteristics and storage information for MOLYKOTE® PA-744 Anti-Friction Coating. Values are not intended as specification limits.

Property Value Unit Method / condition
Product type Anti-friction coating — Heat-cured dry-film lubricant
Technology Organic binder, solids and solvent — Organic resin-solvent dispersion
Solid lubricants Graphite and molybdenum disulfide — Graphite and MoS2 blend
Color Charcoal gray — Typical property
Viscosity 23,000 cP Typical value; test method not stated
Density 1.21 g/mL At 25°C
Flash point 34 °C Typical value; equivalent to 93°F
Recommended cured film thickness 10–20 µm Screen-print application
Usable life 9 months Original sealed container stored above −18°C
Technical properties

After-processing / final-state properties

Typical properties of the cured MOLYKOTE® PA-744 dry lubricating film under the stated preparation and test conditions.

Property Value Unit Method / condition
Cure time 90 min At 180°C
Alternative cure time 60 min At 230°C
Operating-temperature range −75 to 300 °C Cured coating; supplier-listed operating range
Coefficient of friction 0.045 — Polymer tester; 50 cycles, 250 g load, 20 mm stroke
Theoretical coverage 60 ft²/lb At 10 µm cured film thickness
Motor-oil resistance Good — Supplier-documented qualitative performance characteristic
Wear and load performance High wear resistance and load-carrying capacity — Supplier-documented qualitative performance characteristic

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers