PERMABOND 105

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMABOND 105

Main features

  • 5 to 20-Second Fixture Time
  • Low-Viscosity Single-Component Adhesive
  • Hard-to-Bond Plastic and Rubber Bonding

Product Description

PERMABOND® 105 Cyanoacrylate Adhesive is a single-component, low-viscosity, high-purity ethyl cyanoacrylate adhesive developed for rapid bonding of hard-to-bond plastics and rubbers. Surface moisture initiates polymerization when the adhesive is pressed into a thin film between closely fitted parts. The colorless, 100% reactive formulation requires no mixing or heat cure and provides fixture or handling times of 5–20 seconds on documented substrates. Supported materials include natural rubber, Buna N rubber, EPDM, butyl rubber, ABS, PVC, polycarbonate, phenolic materials, and metals.

Key features

  • Rapid fixture performance: Typical fixture or handling times range from 5–20 seconds on documented rubber, plastic, phenolic, and steel substrates.
  • Low-viscosity application: A typical viscosity of 30–50 mPa·s at 25°C supports application into closely fitted joints with a maximum documented gap fill of 0.1 mm.
  • Single-component formulation: The 100% reactive ethyl cyanoacrylate system requires no mixing, solvent evaporation, or heat cure.

Applications / Suitable for

  • Bonding natural and synthetic rubbers, including Buna N, EPDM, and butyl rubber
  • Bonding hard-to-bond plastic components
  • Bonding ABS, PVC, polycarbonate, and phenolic materials
  • Rapid assembly of closely fitted parts
Product Family

PERMABOND 105

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
colorless
Chemistry TypeChemistry Type
Ethyl cyanoacrylate
Specific GravitySpecific Gravity
1.1
Physical Properties
ViscosityViscosity
30-50 mPa.s
Electrical Properties
Dielectric StrengthDielectric Strength
25 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties and processing characteristics of PERMABOND® 105 before full cure. Values are guideline information and do not constitute a specification.

Property Value Unit Method / condition
Chemical composition Ethyl cyanoacrylate — As supplied
Appearance Colorless — As supplied
Viscosity 30–50 mPa·s (cP) At 25°C
Specific gravity 1.1 — Typical
Maximum gap fill 0.1 (0.004) mm (in) Closely fitted bonded joint
Fixture / handling time 5–20 seconds 0.3 N/mm² shear strength achieved; substrate-dependent
Full-strength time 24 hours Temperature, humidity, substrate, surface acidity, and gap can affect cure speed
Technical properties

After-processing / final-state properties

Typical properties and substrate-specific performance of the cured adhesive. Strength results vary with surface preparation and joint gap and do not constitute specifications.

Property Value Unit Method / condition
Shear strength on steel 18–22 (2,600–3,200) N/mm² (psi) ISO 4587
Shear strength on aluminum 6–8 (900–1,200) N/mm² (psi) ISO 4587
Shear strength on PVC >10 (>1,400) N/mm² (psi) ISO 4587; substrate failure
Shear strength on phenolic 12–14 (1,700–2,000) N/mm² (psi) ISO 4587
Impact strength 3–5 (1.4–2.4) kJ/m² (ft·lb/in²) ASTM D950
Hardness 85 Shore D ISO 868
Dielectric strength 25 kV/mm Typical cured-material property
Thermal conductivity 0.1 W/(m·K) Typical cured-material property

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers