PERMABOND 2011

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMABOND 2011

Main features

  • Thixotropic Application Control
  • 5 to 10-Second Fixturing Time
  • One-Part Moisture-Cure Adhesive

Product Description

PERMABOND® 2011 Cyanoacrylate Adhesive is a single-component, thixotropic ethyl cyanoacrylate developed for rapid bonding on vertical and porous surfaces. Its gel consistency supports controlled application with reduced flow, while moisture on the mating surfaces initiates cure after the parts are pressed together. The colorless adhesive fixtures documented steel, Buna N rubber, and phenolic substrates in 5–10 seconds and reaches full strength after 24 hours. It provides a maximum documented gap-filling capability of 0.5 mm and can be used on metals, plastics, elastomers, ceramics, and wood.

Key features

  • Thixotropic gel consistency: Supports controlled application on vertical and porous substrates with a maximum documented gap fill of 0.5 mm.
  • Rapid fixture performance: Reaches 0.3 N/mm² shear strength in 5–10 seconds on documented steel, Buna N rubber, and phenolic substrates.
  • Single-component moisture-initiated cure: Requires no component mixing and develops full strength after 24 hours under documented conditions.

Applications / Suitable for

  • Bonding vertical and porous substrates
  • Bonding metals, plastics, and elastomers
  • Bonding ceramics and wood
  • Rapid assembly of components with gaps up to 0.5 mm
Product Family

PERMABOND 2011

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
colorless
Chemistry TypeChemistry Type
Ethyl cyanoacrylate
Specific GravitySpecific Gravity
1.1
Physical Properties
ViscosityViscosity
30-50 mPa.s
Electrical Properties
Dielectric StrengthDielectric Strength
25 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied and cure-stage properties of PERMABOND® 2011. The technical data sheet identifies these values as guideline information rather than specifications.

Property Value Unit Method / condition
Chemical composition Ethyl cyanoacrylate — Single-component adhesive
Appearance Colorless — As supplied
Viscosity Gel — At 25°C
Specific gravity 1.1 — Typical
Maximum gap fill 0.5 (0.02) mm (in) Documented maximum gap-filling capability
Fixture / handling time 5–10 seconds Time to achieve 0.3 N/mm² shear strength on steel, Buna N rubber, or phenolic
Full-strength time 24 hours Cure speed can vary with temperature, humidity, substrate, surface acidity, and gap
Storage temperature 2–7 (35–45) °C (°F) Allow the adhesive to reach room temperature before opening
Technical properties

After-processing / final-state properties

Typical cured-material and substrate-specific performance data. Bond-strength results vary with surface preparation and joint gap and are not product specifications.

Property Value Unit Method / condition
Shear strength on steel 20–24 (2,900–3,500) N/mm² (psi) ISO 4587
Shear strength on aluminum 8–9 (1,200–1,300) N/mm² (psi) ISO 4587
Shear strength on ABS >8 (>1,200) N/mm² (psi) ISO 4587; substrate failure
Shear strength on PVC >10 (>1,450) N/mm² (psi) ISO 4587; substrate failure
Impact strength 3–5 (1.4–2.4) kJ/m² (ft·lb/in²) ASTM D-950
Hardness 85 Shore D ISO 868
Dielectric strength 25 kV/mm Typical cured-material property
Thermal conductivity 0.1 W/(m·K) Typical cured-material property

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers