PERMABOND 2050

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND 2050

Main features

  • Toughened Structural Bonding
  • 1,200 to 1,800 mPa s Viscosity Range
  • 5 to 15-Second Fixturing Time

Product Description

PERMABOND® 2050 Flexible Cyanoacrylate Adhesive is a medium-high-viscosity, single-component ethyl cyanoacrylate adhesive designed for flexible, semi-porous, and dissimilar-material bonding. Its toughened formulation provides improved peel performance together with resistance to impact, vibration, thermal shock, and thermal cycling. The adhesive has a viscosity of 1,200–1,800 mPa·s at 25 °C and fills gaps up to 0.2 mm. Typical handling strength is reached in 5–15 seconds depending on the substrate, with full strength developing in 24 hours. It is suitable for plastics, elastomers, and metal assemblies where a more flexible instant adhesive bond is required.

Key features

  • Flexible, toughened formulation: Provides improved peel strength and resistance to impact, vibration, thermal shock, and thermal cycling.
  • Fast fixture performance: Typical handling strength is reached in 5–15 seconds depending on the bonded substrate.
  • Controlled medium-high viscosity: A viscosity of 1,200–1,800 mPa·s supports accurate dispensing and gap filling up to 0.2 mm.

Applications / Suitable for

  • Bonding flexible or semi-porous surfaces
  • Bonding dissimilar materials
  • Assemblies exposed to vibration or impact
  • Applications exposed to thermal shock or thermal cycling
  • Bonding plastics, elastomers, and metals
Product Family

PERMABOND 2050

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Liquid
Chemistry TypeChemistry Type
Ethyl cyanoacrylate
ColorColor
Colourless
Specific GravitySpecific Gravity
1.1
Physical Properties
ViscosityViscosity
1,200-1,800 mPa.s mPa.s
Mechanical Properties
Impact StrengthImpact Strength
5-10 kJ/m² mm
Thermal Properties
Thermal ConductivityThermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric StrengthDielectric Strength
25 kV/mm
Maximum gap fillMaximum gap fill
0.2 mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and curing properties. Values are guideline information and do not constitute product specifications.

Property Value Unit Method / condition
Chemical composition Ethyl cyanoacrylate — Single-component adhesive
Appearance Colorless liquid — As supplied
Viscosity 1,200–1,800 mPa·s At 25 °C; equivalent to cP
Specific gravity 1.1 — Typical uncured value
Maximum gap fill 0.2 mm Equivalent source value 0.008 in
Fixture time — steel 10–15 s Time to 0.3 N/mm² shear strength
Fixture time — Buna N rubber 5–10 s Time to 0.3 N/mm² shear strength
Fixture time — PVC 5–10 s Time to 0.3 N/mm² shear strength
Full strength 24 h Typical full-strength development
Technical properties

As-supplied / before-processing properties

Typical uncured and curing properties. Values are guideline information and do not constitute product specifications.

Property Value Unit Method / condition
Chemical composition Ethyl cyanoacrylate — Single-component adhesive
Appearance Colorless liquid — As supplied
Viscosity 1,200–1,800 mPa·s At 25 °C; equivalent to cP
Specific gravity 1.1 — Typical uncured value
Maximum gap fill 0.2 mm Equivalent source value 0.008 in
Fixture time — steel 10–15 s Time to 0.3 N/mm² shear strength
Fixture time — Buna N rubber 5–10 s Time to 0.3 N/mm² shear strength
Fixture time — PVC 5–10 s Time to 0.3 N/mm² shear strength
Full strength 24 h Typical full-strength development

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers