PP-52008G-060-TSF Nylon Peel Ply

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

PP-52008G-060-TSF Nylon Peel Ply

Main features

  • 100% Nylon 6,6 Peel Ply
  • Fine Surface Impression
  • FIN 060 Scoured Heat-Set Fabric

Product Description

PP-52008G-060-TSF Nylon Peel Ply is a 100% nylon 6,6 fabric designed for vacuum-bag composite layups and metal-to-metal bonding structures. The peel ply melts at approximately 480°F (249°C) and leaves a fine surface impression after removal to support subsequent priming and secondary bonding operations. The FIN 060 construction has a scoured and heat-set finish and is available in precision-slit widths of 56 inches or less.

Key features

  • Nylon 6,6 construction: Manufactured from 100% nylon 6,6 fiber with an approximate melting point of 480°F (249°C).
  • Bond-preparation surface: Leaves a fine surface impression suitable for subsequent priming and secondary bonding.
  • Scoured and heat-set finish: FIN 060 is supplied with the manufacturer-designated NAT scoured and heat-set finish.
  • Precision-slit availability: Available in precision-slit widths of 56 inches or less.

Applications / Suitable for

  • Vacuum-bag composite layups
  • Metal-to-metal bonding structures
  • Surface preparation before priming and secondary bonding
Product Family

PP-52008G-060-TSF

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Published product properties. The source states that the information is not to be construed as a specification.

Property Value Unit Method / condition
Material 100% nylon 6,6 fiber — Code 52008
Finish FIN 060 – NAT, scoured and heat-set — Manufacturer finish designation
Fiber melting point Approximately 480 (249) °F (°C) Nylon 6,6 fiber
Roll width 58 (147.3) minimum in (cm) ASTM D3774
Roll length 300 (274.3) maximum yd (m) Published roll format
Weight 1.7 (57.6) minimum oz/yd² (g/m²) ASTM D3776
Finished count – warp 101 (39.8) minimum ends/in (ends/cm) ASTM D3775
Finished count – fill 82 (32.3) minimum picks/in (picks/cm) ASTM D3775
Tensile strength – warp 115 (511.8) minimum lb/in (N) ASTM D5034, grab method
Tensile strength – fill 105 (467.3) minimum lb/in (N) ASTM D5034, grab method
Thickness 0.004–0.005 (0.102–0.127) in (mm) ASTM D1777
pH 4.5–7.0 — AATCC 81
Extractable materials 0.5 maximum % ASTM D2257, petroleum ether

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers